- Poor preheating of materials
- Low firing temperature
- Excessively high discharge rate at the dryer tail
- Insufficient ventilation inside the dryer
- Excessively high rotation speed of the dryer, resulting in an overly short residence time of materials inside the dry mortar dryer
- Poor sealing at the dryer tail with excessive air leakage
- Instrument malfunction
- Ringing or large ball agglomeration inside the dry mortar dryer, leading to insufficient internal ventilation
Possible causes for high tail temperature are as follows:
- High firing temperature
- Excessive ventilation inside the dry mortar dryer
- Burner pipe positioned too far inward
- Insufficient feeding rate or material cut-off at the dry mortar dryer
- Low rotation speed of the dry mortar dryer
- Good preheating of materials with a high decomposition rate
- Instrument malfunction